love the JDM grill!!

Thanks. It's not permanently mounted yet....I've been trying to decide whether to stick with it or go back to the OEM grille.

It looks a little cleaner and it is different...I've just been trying to decide which grille I like better.

Link to comment
Share on other sites

Keep them both. I have the same JDM-style grill on mine, but keep the original stored away with my other original parts so I can sell it in stock trim (if I ever get desperate enough)

Link to comment
Share on other sites

Steve, did you find that the mounting points lined up with where your old grille attached?

Either my front end got tweaked at some point, or the mount points for the grille are off by a bit. The old grille fits, of course, but then again it's not exactly straight, either....

Link to comment
Share on other sites

Hi Brian,

Only three of the five mounting points lined up well--the bottom middle one, and the two on the top upper corners. Even those two required some tweaking. The bottom outer two mount points weren't even close. But, when it's all installed it's nearly impossible to tell unless you're obsessive or within a foot of it, so it's not a big deal.

What are you using to buff/polish after your wetsanding?

Link to comment
Share on other sites

......when it's all installed it's nearly impossible to tell unless you're obsessive or within a foot of it, so it's not a big deal.

What are you using to buff/polish after your wetsanding?

Obsessive? Over a Z car? I resemble that remark.....!

I didn't do the buffing myself, the guys at the shop did that after they wet sanded. Some of the other guys might have some recommendations on what kind of buffing compound to use, though....

Link to comment
Share on other sites

I use 3 compounds total cost of $90-110. 3M extra cut for removing 1500-2000 sand marks. Then 3M swirl mark remover followed my 3M finish it or finesse it. Afterwards I hand wax with Mcquires gold carnubeau (sp?)

I also use a variable high speed buffer. Usually buff at about 2000-3000RPM. I use a tericloth pad for the extra cut, then a coarse foam pad for swirl mark and a fine foam pad for the final compound

Link to comment
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
  • Recently Browsing   0 members

    • No registered users viewing this page.
  • Who's Online   1 Member, 0 Anonymous, 713 Guests (See full list)

×
×
  • Create New...

Important Information

By using this site, you agree to our Privacy Policy and Guidelines. We have placed cookies on your device to help make this website better. You can adjust your cookie settings, otherwise we'll assume you're okay to continue.